HEAT RESISTANT ALLOYS FOR GENERAL APPLICATIONS

ALLOY NAME

ASTM Spec

Max. Temp.

Description

HC

A 297

2000 º F
1090º C

Good sulfur and oxidation resistance, minimal mechanical properties.

HD

A 297

2000 º F
1090º C

Excellent oxidation and sulfur resistance, plus weldability.

HE

A 297

2000 º F
1090º C

Higher temperature and sulfur resistance capabilities than HD.

HF

A 297

1600 º F
870º C

Excellent general corrosion resistance to 1500ºF (815ºC), with moderate mechanical properties.

HH

A 297, A 608

2000 º F
1090º C

Good strenght and oxidation resistance at 1400-1800ºF (760-980ºC).

HI

A 297

2000 º F
1090º C

Improved oxidation resistance compared with HH.

HK

A 297, A 608

2100 º F
1150º C

Better strenght and oxidation resistance than HH, working range up to 1900ºF (1050ºC).

HL

A 297

1800 º F
980º C

Improved sulfur resistance compared with HK.

HN

A 297

2000 º F
1090º C

Very high strenght at high temperatures.

HP

A 297

2000 º F
1090º C

Resistant to both oxidizing and carburizing atmospheres at high temperatures.

HT

A 297, A 608

2100 º F
1150º C

Good thermal shock/fatigue resistance. Good carburizing resistance.

HU

A 297, A 608

2100 º F
1150º C

Improved mechanical properties over HT.

HW

A 297, A 608

1800 º F
980º C

High thermal shock/fatigue and carburizing resistance with higher nickel.

HX

A 297, A 608

2100 º F
1150º C

Resistant to hot corrosive gas under cyclic conditions without cracking or wraping.

Botón